WI3000-PD11 COPPER PLATING

Total questions: 10

Worksheet time: 10mins

Name
Class
Date
1.

Which is below equipment used in copper plating line:

i. Jig & Jib hoist

ii. Anode and cathode

iii. Temperature Controller (Calibrated)

iv. Laboratory apparatus

a)

i, ii and iii

b)

i, ii and iv

c)

i, iii and iv

d)

All of the above

2.

How the operator knows if the chemical is contaminated?

a)

By the color of the chemical

b)

By the titration report

c)

From the smell of the chemical

d)

From the product plated

3.

The frequency of performing titration test on specified tanks to verify concentration of solution are:

a)

Prior to copper for each process

b)

After adding chemical or water

c)

After change of chemical

d)

All of the answer

4.

Determination of actual chemical concentration from each solution tank shall be calculated by using specified formula in the _________ and shall be verified by QA/QC Manager and/or chemist and/or QAQC Supervisor.

a)

Titration Test Report

b)

Daily production form - Copper Plating

c)

Current and Time for Copper Plating

d)

Plating Thickness Report

5.

In case that the symptoms of poor conductivity are observed, such as plating peeling off, no plating at all, abnormal plating colour, check the following:

i. Flight bar is over-heated.

ii. Additives and chemicals in the copper plating tanks are out of balance.

iii. Too much sediment or contamination.

iv. Current values displayed at the digital regulator monitor are not consistent once the flight bar is loaded.

a)

i, ii and iii

b)

i, ii and iv

c)

i, iii and iv

d)

All of the above

6.

If plating thickness is observed to have an irregularity or found out of tolerance, check following:

i. Current is not consistent (Current shall be measured by using Clamp meter for verification)

ii. Improper agitation

iii. Improper loading, i.e. the anode bar is not at the center of intended plated item.

iv. Anode has worn off

a)

i, ii and iii

b)

i, ii and iv

c)

ii, iii and iv

d)

All of the above

7.

Thickness of the copper plating shall be checked on the actual __________ or the flat area in front of the seal.

a)

Pin thread crest

b)

Box thread crest

c)

Box thread flank

d)

Seal shoulder

8.

Arrange the process of normalization:

i. Press "Zero" on the Fischer gauge

ii. Check for 5 times

iii. The gauge is ready to be used to check copper plated couplings

iv. Successful Normalization finished screen will appear

v. Place the Probe on the thread crest material to be checked

vi. Press "Enter" on the Fischer gauge

a)

i > ii > iii > iv > v > vi

b)

i > iii > ii > vi > v > iv

c)

i > v > ii > vi > iv > iii

d)

i > v > iv > iii > ii > vi

9.

To remove the hard-bonding of nickel and copper on the surface of the chrome material, a mixture of __________ is used.

a)

10% Nitric acid with 90% of water

b)

100% of water with 50% Nitric acid

c)

50% of water with 100% of Nitric acid

d)

50% Nitric acid with 50% of water

10.

Water pressure test Pressure: _________ bar.

a)

150

b)

120

c)

110

d)

100