WorksheetsQUIZ CHAPTER 3 - WET LAYUP
Total questions: 20
Worksheet time: 16mins
There are two (2) types of wet layup commonly known are
hand lay-up and spray-up.
TRUE
FALSE
These statement are true about wet layup EXCEPT..
I. Most common and basic techniques in composite
process.
II. It is cheap, labor intensives and most versatile for the
product that do not require high precision and high
properties.
III. Curing techniques by autoclave cure
IV. Theses processes can be applied on a small product such as water tank up to big scale product as leisure yard.
I, II, III
I, II, IV
II, III, IV
MEKP stands for
Methyl Ethanol Ketone Peroxide
Methyl Ethylene Ketone Peroxide
Methyl Ethyl Ketone Peroxide
The spray-up process is approximately similar to hand lay-up method EXCEPT
Large and complex item can be produced
the use of sprayed chopped glass from continuous fiber with along with catalyzed resin on top of the gel coat layer
Any material that will hold it shape can be used as mold form
Cleaning the uncured polyester resin from brushes and tools can be done using acetone
TRUE
FALSE
It has advantages of having greater strength and adhesion, strong adhesion to hardwood, metal and glass, lower shrinkage and chemical resistance . This statement is referring to
Polyester
Epoxy
Acetone
First step when working in open mold is application of release material to the mold. This statement is referring to...
I. Wax
II. PVA
III. Gelcoat
IV. Release papers and release films
I, II, III
I, II, IV
II, III, IV
The resin to glass ratio is to about 1:2
TRUE
FALSE
Spray Up equipment are available in three (3) types.
TRUE
FALSE
The “green” stage is where the laminate is fully cured, and the trimming process at the edges is advisable to be done at this stage.
TRUE
FALSE
The advantages of using open hand lay-up and spray up process are as below statement EXCEPT
Design flexibility
The start-up lead time and cost are minimal
Both good surface are obtained
If practice the wet laminating hand lay-up process to fabricated the product, which fiber appropriate to used.
I. Roving
II. CSM 300
III. CSM 450
IV. Woven Roving 600
I, II, III
I, II, IV
II, III, IV
Calculate the total surface area for that product
0.25 m2
0.30 m2
0.45 m2
How many fiber CSM 300 will be used to produce the products through hand lay-up process referring to below diagram.
60.5 gram
75.0 gram
112.5 gram
How many fiber WR 600 will be used to produce the products through hand lay-up process referring to below diagram
75.0 gram
112.5 gram
150.0 gram
Release agent act as a?
Curing agent for composite product
To make sure product can demold from mould
Hardener agent to the resin
Fiber glass is expensive than carbon fiber.
TRUE
FALSE
Resin will hot and gel suddently if we add MEKP too much
TRUE
FALSE
Resin will gel like usual without MEKP added
TRUE
FALSE
Referring to below diagram, calculate the total surface area for that product.
0.40 m2
1.04 m2
1.20 m2