Font size
WorksheetsCHP18
Total questions: 91
Worksheet time: 46mins
What does a whirling hygrometer/psychrometer measure?
Rain
Wind Speed
Relative humidity
What are the two types of steel temperature gauges?
Magnetic and anti-magnetic
Magnetic and digital thermometer
Medium and antimagnetic
Medium and digital thermometer
Condensation occurs when ____________ is reached
An air temperature less than 0°C (32°F)
A humidity greater than 90%
The dew point
A steel temperature of less than 0°C (32°F)
If a painting inspector is not available, environmental conditions should be checked ____________
By nobody
By supervisor or foreman
Only when the humidity is high
Only when 2-pack paint is used
What situation would cause environmental condition checks to be more frequent?
Different product being applied
Increasing air temperature
Decreasing air temperature
Increasing relative humidity
If the temperature of a steel structure falls during the night, there is a risk of ____________
Coating discoloration
Condensation
Coating detachment
Blistering
Information on relative humidity, dew point, and overcoating times are shown on ____________
Safety data sheet
International Standard
Product data sheet
Code of practice
The environmental condition criteria should be found in the?
Coating specification
Risk Assessment
Method Statements
Paint Tin Label
Dew point can be calculated from ____________
Wet and dry bulb temperatures
Steel temperature and wet bulb temperature
Steel temperature and dry bulb temperature
Relative humidity and steel temperature
Which of the steel temperature gauges, magnetic and digital, will give almost instantaneous results?
Electronic
Magnetic and anti-magnetic
Both
Neither
Currently, NACE and ____________ produce joint standards.
DIN
BS
ISO
SSPC
The Norsok M501 standard is mainly used in the ____________ industry.
Highways
Aerospace
Oil and gas
Marine
What does BS stand for?
British Stores
British Standards
British Steel
Big Sections
What does ISO stand for?
International Standard Organisation
International Stable Oxygen
Internal Standards Organisation
In Stable Oxygen
What does SSPC stand for?
Steel Surfaces Painting Certificates
The Society for Protective Coatings
Stainless Steel Paint and Coating
Stainless Steel Painting Council
What does NACE stand for?
National Association of Corrosion Engineers (NACE International)
National Assembly Coat Engineers
Names Assembled Corrosion Engineers
Nothing Assembles Concrete Energy
What does ASTM stand for?
American Steel Testing Metal
Always Steel Testing Metal
American Society Testing and Materials (ASTM International)
American Society Testing Metals
ISO standards are compiled by ____________.
Representative experts from a number of countries
Experts at headquarters in Geneva
Individuals who are experts in the subject
A committee of experts from NACE and SSPC
An SSPC standard that is universally adopted for dry film thickness is ____________.
SSPC PA1
SSPC PA2
SSPC-PA Guide 4
SSPC-PA Guide 5
An ISO standard widely specified for surface preparation is ____________.
ISO 8502-3
ISO 4628
ISO 8501-1
ISO 8503-1
Which SSPC standard is for industrial blast cleaning?
SP6
SP8
SP10
SP14
In SSPC Vis 1, which rust grade contains both mill scale and rust?
A
B
Curing reaction
D
NACE and SSPC have how many levels of surface preparation by abrasive blast cleaning?
Four
Three
Six
Five
Visual standards and guides exist for Waterjetting?
True
Only on cast iron surfaces
Only on stainless steel surfaces
Only on wood surfaces
The SSPC standard for power tool cleaning to bare metal is ____________.
SP2
SP3
SP11
SP13
The main visual standard for surface preparation used in Europe is?
ISO 8500
ISO 8505
ISO 8501
ISO 8880
How many rust grades are within ISO 8501?
2
4
6
8
What is the missing standard from the list SA1, SA2, SA3?
SA2.5
SA2.55
SA2.3
SA2.9
Very thorough hand and power tool cleaning is designated?
St2
St3
St4
St5
How is the visual standard to be used?
Held close to the surface to be assessed
Held away from the surface and illuminated
Referred to in the office before an inspection
Only used in the case of a dispute
The process of checking that the work is carried out in accordance with the specification is called?
Quality assurance
Quality audit
Quality control
Quality statement
The paint specification usually forms part of a contract.
Yes, generally
No, never
Only in the petrochemical industry
Only in the offshore industry
If there is no paint specification, the ____________ should be referred to for application details.
Manager
Foreman
Product safety data sheet
Product data sheet
The document that details why and how inspections are conducted is called?
Inspection log
Inspection test plan
Paint specification
Paint data sheet
The ____________ of the paint specification should be checked to confirm it is the current edition.
Revision status
Date
Standard reference
Paint data sheet
The paint specification may specify selective coating manufacturers.
No, never
Yes
Only for tank lining works
Only for sub-sea work
The paint specification usually specifies the standard of preparation.
Yes, usually
Never
Only for pitted steel
Only on stainless steel
Paint specifications should have a revision status.
Yes
No
Only on large jobs
Only on small jobs
Paint specifications often refer to standards such as ISO, ASTM, etc.
Never, stand-alone documents
Yes, often
Only for large jobs
Only for marine works
Environmental conditions, film thickness, types of equipment, standards, mixing, storage are a few items to be found in a typical paint specification.
No
Yes
Only on tank lining jobs
Only on sub-sea jobs
The ____________ is also called resin, vehicle, or polymer.
Pigment
Solvent
Binder
Paint
Solvents can be organic or ____________ based.
Inorganic
Water
Synthetic
Viscous
____________ provide color and opacity together with durability, hardness, mechanical strength, and in some cases rust inhibiting or antifouling properties.
Solvent
Additive
Pigment
Binder
The ____________ imparts adhesion and strongly influences properties such as gloss, durability, flexibility, and toughness.
Solvent
Pigment
Binder
Extender
The ____________ imparts adhesion and strongly influences properties such as gloss, durability, flexibility, and toughness.
Solvent
Pigment
Binder
Extender
An example of a pigment with a laminar structure is ____________.
Barytes
China clay
Mica
Talc
Paints are often referred to by the type of ____________.
Pigment
Solvent
Curing reaction
Binder
Pigments, extenders, resin, ____________, and additives are mixed together to form a paste.
Solvents
Air
Gas
Water
All coatings should have a ____________ number.
Colour
Health
Batch (generally found on the label)
Safety
Pigments ____________.
Always organic
Soluble in the binder
Always inorganic
Can be organic or inorganic
Paint mills are used to ____________ during paint manufacture.
Generate heat
Disperse the paint components
Keep the mixture cool
Adjust the viscosity
Information on the voltage to be used for porosity testing should be obtained from ____________.
The site manager
The product data sheet
The paint manufacturer
The safety data sheet
I am an Intrinsically safe (no batteries) type gauge.
Magnetic gauge
Electronic gauge
Ferrous gauge
Non-magnetic gauge
Calibrated thickness shims should be used with DFT gauges before use.
True
Not True
Only on old equipment
Only on repaired equipment
The coating applicator should carry out ____________ tests during application.
Surface profile on blasted substrates
Dry film thickness
Relative humidity
Wet film thickness
Wet film combs are available in steel, aluminum, and ____________.
Gold
Glass
Plastic
Paper
Plastic combs are generally 'used ____________ ' only as the paint/solvent can melt the plastic.
Once
Frequent
Often
Unlimited
Electronic steel temperature gauges can be used ____________.
Slowly
When warmed up
On stainless steel only
Instantaneously
Steel temperature gauges need ____________ to ____________ minutes to stabilize before use.
60-70
50-60
10-20
20-30
Dew meters will measure steel temperature, relative humidity, and ____________ point.
Damp
Dew
Steel
Moisture
A surface profile gauge measures the?
How flat a surface is
How smooth a surface is
How curved a surface is
Surface profile on blasted substrates
The documentation on a coatings job is generally completed by the?
Client
Painter
Stores person
Supervisor, manager, or inspector
The coating specification should be available to ____________.
Painters only
Client only
Everybody
Nobody
It is vitally important to keep a site ____________ or log information on events.
Cabin
Fresh safe
Diary (or log)
Inspection tool
A site diary can be used in the event of a ____________.
Fire
Power cut
Prize
Dispute
Environmental conditions shall be recorded where?
On a wall chart
On a notepad
In the daily log
In the daily log but only if they are outside the specification
Inspection equipment should have a unique identity number to assist with ____________.
Ownership
Storage location
Traceability
Calibration
The daily inspection report should be signed and ____________.
Sealed
Printed
Dated
Posted
Overcoating times and curing times are available on the ____________.
Safety data sheet
Product data sheet
Paint tin
Specification
The plant and equipment should be logged on a ____________ basis.
Regular
Annual
Daily
Bi-annual
To enable planning of the work, an up-to-date ____________ should be maintained.
Weather forecast
Set of meeting notes
Work program
Progress report
The standard contains four languages: English, French, Swedish, and __________?
Arabic
Spanish
Polish
German
The standard is to be used for __________ assessment of rust grades and surface preparation grades?
Visual
Comparison
Good
Possible
The standard includes _______ high-quality photographs of rust grades, abrasive blast cleaned grades, and hand and power tool cleaning grades?
38
28
18
8
Photographic illustrations include flame _________ preparation?
Washing
Dusting
Warming
Cleaning
24 blast-cleaned photographs were taken from the original __________ Standard SIS 05 59 00 - 1967?
Danish
Swedish
Norwegian
French
How many rust grades exist in the standard?
2
3
4 (A, B, C, and D)
8
Steel surfaces largely covered with adhering mill scale but little, if any, rust, which grade am I?
B
C
A
D
Steel surface on which the mill scale has rusted away and on which general pitting is visible under normal vision, which grade am I?
B
C
A
D
All surface preparation standards are prefixed Sa, __ and F1?
St
Sb
Sc
Sa
All blast inspection should be conducted without magnification?
True on new steel only
True on pitted steel only
Not true
True
ISO 8501 specifies a series of preparation grades for steel surfaces after __________ removal of previous paint coatings?
Partial
Some
Localised
Remedial
ISO 8501 is applicable to surfaces prepared for painting by methods such as blast cleaning, hand and power tool cleaning, and machine __________?
Abrading
Washing
Cleaning
Scuffing
The degree of degradation which may be found on previously coated surfaces shall be assessed in accordance with ISO _______, Parts 1 to 6?
2846
4682
8264
4628
Each preparation grade is designated by the appropriate letter Sa, St, or ______?
Na
Ma
P
Nr
Surface preparation by localised blast cleaning is designated by the letters __ Sa.?
P
S
A
B
The adhesion of existing coatings may be checked by knife, by a cross-cut test, or a portable apparatus for pull-off adhesion.?
True
Not True
True for old coatings only
True for new coatings only
The newly applied coatings should be __________ with the existing coatings.?
Painted
Coated
Over coated
Compatible
Iron oxide shop primer prior to surface preparation with localised blast cleaning, what am I?
A Sa2½
P Sa2½
C Sa2½
P Sa2
P Ma picture shows typical cases of localised machine abrading using repair work to ______ in a power station.?
Welds
Pipes
Tubes
Steel
P Ma picture shows typical case of localised machine abrading repair work to the upper sides of a ______ cover.?
Door
Hatch
Ship
Steel